Key improvements in the machining of difficult-to-cut aerospace superalloys

Article Properties
Cite
Ezugwu, E.O. “Key Improvements in the Machining of Difficult-to-Cut Aerospace Superalloys”. International Journal of Machine Tools and Manufacture, vol. 45, no. 12-13, 2005, pp. 1353-67, https://doi.org/10.1016/j.ijmachtools.2005.02.003.
Ezugwu, E. (2005). Key improvements in the machining of difficult-to-cut aerospace superalloys. International Journal of Machine Tools and Manufacture, 45(12-13), 1353-1367. https://doi.org/10.1016/j.ijmachtools.2005.02.003
Ezugwu E. Key improvements in the machining of difficult-to-cut aerospace superalloys. International Journal of Machine Tools and Manufacture. 2005;45(12-13):1353-67.
Refrences
Refrences Analysis
The category Technology: Mechanical engineering and machinery 16 is the most frequently represented among the references in this article. It primarily includes studies from Wear The chart below illustrates the number of referenced publications per year.
Refrences used by this article by year
Citations
Citations Analysis
The first research to cite this article was titled Some considerations on tool wear and workpiece surface quality of holes finished by reaming or milling in a nickel base superalloy and was published in 2007. The most recent citation comes from a 2024 study titled Some considerations on tool wear and workpiece surface quality of holes finished by reaming or milling in a nickel base superalloy . This article reached its peak citation in 2020 , with 68 citations.It has been cited in 167 different journals, 17% of which are open access. Among related journals, the The International Journal of Advanced Manufacturing Technology cited this research the most, with 74 citations. The chart below illustrates the annual citation trends for this article.
Citations used this article by year